Bambanci Tsakanin RA Copper da ED Copper

Sau da yawa ana tambayarmu game da sassauci. Tabbas, me yasa za ku buƙaci allon "sauki"?

"Shin allon lanƙwasa zai fashe idan aka yi amfani da ED copper a kai?"

A cikin wannan labarin, muna son mu binciki abubuwa guda biyu daban-daban (ED-Electrodeposited da RA-rolled-annealed) kuma mu lura da tasirinsu ga tsawon rayuwar da'irar. Duk da cewa masana'antar sassauƙa ta fahimce mu sosai, ba mu sami wannan muhimmin saƙo ga mai tsara hukumar ba.

Bari mu ɗan yi bitar waɗannan nau'ikan foil guda biyu. Ga yadda aka lura da RA Copper da ED Copper:

ED COPPER VS RA COPPER

Sassauci a cikin jan ƙarfe yana fitowa ne daga abubuwa da yawa. Tabbas, mafi siririn jan ƙarfe shine mafi sauƙin sassauƙa. Baya ga kauri (ko siririn), ƙwayar jan ƙarfe kuma tana shafar sassauci. Akwai nau'ikan jan ƙarfe guda biyu da ake amfani da su a kasuwannin PCB da kewaye masu lanƙwasa: ED da RA kamar yadda aka ambata a baya.

Naɗewar Anneal Copper Foil (RA jan ƙarfe)
An yi amfani da jan ƙarfe sosai a masana'antar kera da'irori masu lankwasa da kuma masana'antar kera PCB mai lankwasa tsawon shekaru da dama.
Tsarin hatsi da saman santsi ya dace da aikace-aikacen kewaye masu ƙarfi da sassauƙa. Wani fanni mai ban sha'awa tare da nau'ikan tagulla da aka naɗe yana cikin sigina da aikace-aikacen mita mai yawa.
An tabbatar da cewa rashin kyawun saman jan ƙarfe na iya yin tasiri ga asarar shigarwar mai yawan gaske kuma santsi saman jan ƙarfe yana da amfani.

Tsarin Tagulla na Electrolysis (ED jan ƙarfe)
Tare da jan ƙarfe na ED, akwai bambancin foils iri-iri dangane da rashin kyawun saman, magani, tsarin hatsi, da sauransu. A matsayin gabaɗaya, jan ƙarfe na ED yana da tsarin hatsi a tsaye. Tagulla na ED na yau da kullun yawanci yana da babban matsayi ko saman da ba shi da ƙarfi idan aka kwatanta da jan ƙarfe na Rolled Annealed (RA). Tagulla na ED yana da rashin sassauci kuma baya haɓaka ingantaccen sigina.
Tagulla ta EA ba ta dace da ƙananan layuka da kuma rashin juriya ga lanƙwasawa ba, don haka ana amfani da tagullar RA don PCB mai sassauƙa.
Duk da haka, babu wani dalili da zai sa a ji tsoron ED jan ƙarfe a cikin aikace-aikacen da ke aiki.

Takardar jan ƙarfe -cHINA

Duk da haka, babu dalilin jin tsoron jan ƙarfe na ED a cikin aikace-aikacen masu ƙarfi. Akasin haka, shine zaɓin gaskiya a cikin aikace-aikacen masu amfani da sirara, masu sauƙi waɗanda ke buƙatar ƙimar zagayowar mai girma. Abin damuwa kawai shine kula da hankali kan inda muke amfani da faranti na "ƙari" don tsarin PTH. RA foil shine kawai zaɓin da ake samu don nauyin jan ƙarfe mai nauyi (sama da oza 1) inda ake buƙatar aikace-aikacen yanzu mai nauyi da lanƙwasa mai ƙarfi.

Domin fahimtar fa'idodi da rashin amfanin waɗannan kayan guda biyu, yana da mahimmanci a fahimci fa'idodin farashi da ingancin waɗannan nau'ikan foil ɗin jan ƙarfe guda biyu, da kuma, kamar yadda yake da mahimmanci, abin da ake samu a kasuwa. Mai ƙira yana buƙatar ba wai kawai ya yi la'akari da abin da zai yi aiki ba, har ma ko za a iya siyan sa a farashin da ba zai fitar da samfurin ƙarshe daga kasuwa ta hanyar farashi ba.


Lokacin Saƙo: Mayu-22-2022